Supplier: | ADW |
Drying time: | 1 mm layer in temp. 20°C approx. 6 hours |
Number of layers: | 1-3 |
Quantity per Pallet: | 48 pcs. |
Application temperature: | from +5°C to +30°C |
Package: | 10 kg |
Usage: | 0,4-0,8 kg/m2/layer |
Weight: | 10 kg |
Dysperbit is intended for:
- renovation and maintenance of old roofing
- making seamless roof coatings based on asphalt felt papers,
- making a seamless waterproofing layer on all vertical and horizontal planes, with the use of matrices strengthening the coating and facilitating its arrangement (e.g. polypropylene mesh, glass veils and fabrics, polyester nonwovens)
- waterproofing and anti-moisture insulation of all types, incl. ceilings, strip foundations, floors (e.g. basements, bathrooms), balconies, terraces, swimming pools.
PRODUCT ADVANTAGES:
- does not contain organic solvents
- product & amp; ldquona cold "- ready to use
- easy to use - minimal effort
- possibility of laminating with reinforcement inserts made of technical fabrics
- does not react with polystyrene, possibility of use together with materials
not resistant to organic solvents and their vapors
- easy to transport horizontally and vertically
SURFACE PREPARATION
The surface should be even , clean, free of dust and dust. Concrete, gypsum, ceramic surfaces etc. should be primed with DYSPERBENT IZOPLAST solution diluted with water in the ratio 1: 1
Insulating coating
Apply with a brush on the prepared surface. Work should be carried out in the temperature above 5 ° C and rainless weather (outside). The drying time for a 1 mm thick layer at 20 ° C is approx. 6 hours. During this period, the coating is not resistant to water. Depending on the needs, make from 1 to 3 layers. Apply the next layer after the previous one is dry.
Lamination: apply the DYSPERBENT IZOPLAST mass on the prepared surface, then place the fabric and saturate with the mass. After drying, apply additional layers.
On roofs and surfaces exposed to direct sunlight, in order to increase the durability of waterproofing, the top layer can be covered with quartz sand or mineral coloring sprinkles.
Mass consumption, depending on the substrate and workmanship. , ranges from 0.4-0.8 kg / m? one layer of waterproofing.